Evaluation Of The Thermoluminescence Kinetic Paramters Of Zinc-Borosilicate Glass After Gamma-Irradiation

Up until now, there was no detailed study concerning the kinetic parameters of zinc-doped borosilicate glass thermoluminescent (TL) material. A significant TL peak was observed upon gamma irradiating the samples at around 185 deg C. Evaluating activation energy (E), frequency factor (s), and order of kinetics (b) were conventionally obtained by peak shape (PS) method, repeated initial rise (RIR) and variable heating rate (VHR) methods. The obtained results indicated that he zinc-doped borosilicate glass glow curve after gamma irradiation is legitimately a superposition of seven interfered glow peaks. Therefore, we cannot use computerised glow curve deconvolution (CGCD) method alone in determining the kinetic parameters in this case. Additive dose (AD), repeated initial raise (RIR) and variable heating rate (VHR) methods, together with computerised deconvolution method by using the TolAnal software have been applied to determine the kinetic parameters of zinc-borosilicate glass due to the existence of several nearby overlapped peaks.

Author
H A Soliman Et Al
Origin
Nat Inst For Standards, Ionizing Radiation Lab, Cairo, Egypt
Journal Title
Int J Appl Glass Science 9 1 2018 99-104
Sector
Special Glass
Class
S 4452

Request article (free for British Glass members)

Evaluation Of The Thermoluminescence Kinetic Paramters Of Zinc-Borosilicate Glass After Gamma-Irradiation
Int J Appl Glass Science 9 1 2018 99-104
S 4452
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.