Evaluation Of Chemically Tempered Soda-Lime-Silica Glass By Bend Testing

The objective of this paper is to demonstrate that the surface of glass can be strengthened by ion exchange, by preparing ion-exchanged glass and comparing its failure characteristics to as-received glass.

Author
L R Bunnell & S W Piippo
Origin
Southridge High School & Richland High School, Washington, Usa
Journal Title
Std Experiments In Eng Mat Sci & Technol 1 July 1997 55-63