Energetics Of The Charge-Coupled Substitution Si4+ - Na+ + T3 In The Glasses Nato2-Sio2 (T = Al, Fe, Ga, B)

Heats of solution in molten 2PbO.B2O3 at 973 K are reported for glasses xNaT3+O2-(1-x)SiO2 for T = Fe, Ga.

Author
J J De Yareo, A Navrotsky, D B Dingwell
Origin
Princeton University, Universitat Beiruth
Journal Title
J Am Ceram Soc 1990 73 7 2068-2072