Electron Paramagnetic Resonance And Optical Absorption Spectra Of Vo2+ Ions In Alkali Cadmium Borosulphate Glasses

The electron paramagnetic resonance spectrum of 9.205 GHz is examined at 300K for a series of VO2+ ion doped R2SO4-B2O3-CdSO4 (R = Li, Na, K or Cs) glasses and the spin Hamiltonian parameters, dipolar hyperfine coupling parameter, K, are evaluated from the spectra.

Author
A S Rao Et Al
Origin
Sri Venkatesware University, India
Journal Title
Phys & Chem Glasses 1992 33 1 1-4
Sector
Special Glass
Class
S 617