Electrodiffusion Of Alkali Ions In Alkali Niobophosphate Glasses And Glass-Forming Melts

Electrical conductivity of Li(Na,K)2O-Nb2O5-P2O5 glasses and glass forming melts has been measured in a wide temperature range (298-1173 K). Logarithm of the pre-exponential factor and activation energy of migration have been determined. Mixed alkali effect has been observed in niobophosphate glass-forming melts.

Author
V A Markov Et Al
Origin
Unknown
Journal Title
Int J Appl Glass Sci January 2019 69-74
Sector
Special Glass
Class
S 4499