Electrochemical Measurement Of Oxygen Activity In Lead Glass By Means Of A Stabilized Zro2 Sensor. Part 2. Determination Of The Equilibrium Constants In The Redox Systems Arsenic And Antimoney

The effect of antimony and arsenic systems on lead glass refining has been demonstrated by using chemical analysis and electrochemical measurement to determine the equilibrium constant and standard thermodynamic quantities.

Author
O Lafroukhi Et Al
Origin
Universite De Nancy, Cristalleries De Baccarat
Journal Title
Glastech Ber 1991 64 11 281-290
Sector
Domestic glass
Class
D 128

Request article (free for British Glass members)

Electrochemical Measurement Of Oxygen Activity In Lead Glass By Means Of A Stabilized Zro2 Sensor. Part 2. Determination Of The Equilibrium Constants In The Redox Systems Arsenic And Antimoney
Glastech Ber 1991 64 11 281-290
D 128
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.