Electrical Conductivity Of The Melts In The K20-Pb0-Si02 System

The specific conductivity of melts int he K20-Pb0-Si02 system was measured as a function of temperature and composition within their glass forming regions. Because conductivity is very sensitive to composition changes it can be considered as an appropriate method for choosing a good quality, stable glass. Leaching tests were also performed on the studied glasses in order to establish the limiting conductivities of the melts.

Author
M Constantinescu Et Al
Origin
Romanian Academy, Inst Of Physical Chemistry
Journal Title
Glass Technology 38 2 1997 62-64
Sector
Special Glass
Class
S 1148

Request article (free for British Glass members)

Electrical Conductivity Of The Melts In The K20-Pb0-Si02 System
Glass Technology 38 2 1997 62-64
S 1148
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.