Electrical Conductivity Measurements In High Temperature Glasses (In Italian)

Modern glass furnaces using dipped electrodes need a good knowledge of electrical glass properties at high temperatures, namely as regards electrical conductivity. In the last decade several methods have been proposed for measuring electrical conductivity. This paper considers some of these methods and introduces a new one with the aim to study polarisation mechanisms.