Electrical Conduction In Magnesium Phosphate Glasses Containing Heavy Water

The relation between dc conductivity and the concentration of protons or deuterons was investigated in 45MgO.55P2O5 (in mol %) glases containing small amounts of "water".

Author
H Hosono, T Kamae, Y Abe
Origin
Nogoya Institute Of Technology
Journal Title
J Am Ceram Soc 1989 72 2 294-297