Electrical Conduction In Bi203-B203 Glassy Systems

Five glasses of (Bi203)x-(B203)1-x, x=0.06-0.26, have been prepared by melting in an open crucible. The density, thermal analysis and FT-IR spectra were measured. The softening temperature decreased with the bismuth oxide content in the sample. The x-ray diffraction confirmed the amorphous nature for the prepared samples.