Effects Of Dissolved Nitrogen And Carbon On Container Glass Compositions

Additions of Si3N4 and SiC were made to two commercial glass compositions. The highest rate of improvement of mechanical properties was associated with very low levels of nitrogen content. (abstract only)

Author
C C Sorrell Et Al
Origin
Univerisyt Of New South Wales
Journal Title
J Australian Ceram Soc 1988 24 1 35
Sector
Container glass
Class
C 171