Effects Of (B203, P205) Additives On Microstructural Development And Phase-Transformation Kinetics Of Stoichiometric Cordierite Glasses

The microstructural development and phase-transformation kinetics of stoichiometric cordierite glasses containing B203 and/or P205 additives were highly affected by the microstructural characteristics of the u-cordierite and the type of additives. The addition of B203 tended to cause the formation of u-spherulitic dendrites with thin dendritic arms, which promoted the formation of a-cordierite, either from crystallization of the residual glass or from transformation of u-cordierite. P205 had the opposite effect: Increasing the temperature increased the growth rate of a-cordierite more than that of u-cordierite.

Author
J Wu & S Hwang
Origin
National Tsing Hua University, Taiwan
Journal Title
J Am Ceram Soc 83 5 2000 1259-1265
Sector
Special Glass
Class
S 1922

Request article (free for British Glass members)

Effects Of (B203, P205) Additives On Microstructural Development And Phase-Transformation Kinetics Of Stoichiometric Cordierite Glasses
J Am Ceram Soc 83 5 2000 1259-1265
S 1922
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.