The Effects Of Atmospheres On Volatilization And Surface Tension

The effects of atmospheres on the volatilization and surface tension of TV panel and other silicate glasses were studied by measuring the weight loss and wetting angle of small glass samples heat treated in an atmosphere-controlled furnace.

Author
H Jiant, W C Lacourse
Origin
Alfred University, Usa
Journal Title
Ceramic Trans 82 1998 233-238
Sector
Special Glass
Class
S 1611a

Request article (free for British Glass members)