The Effect Of Process Parameters On The Stability Of Molybdenum Electrodes In Glass-Melting Furnace

An integrated estimate of raw materials, batches and compositions of container glass is carried out with respect to their efficiency in electric melting. A substantial effect of the redox parameters of the materials and the batch on the glass melting process and the corrosion of molybdenum electrodes is demonstrated in this paper. Recommendations for the improvements of container glass production technology are given.

Author
N I Minko Et Al
Origin
Unknown
Journal Title
Glass & Ceramics 57 9-10 2000 333-337
Sector
Container glass
Class
C 3185

Request article (free for British Glass members)

The Effect Of Process Parameters On The Stability Of Molybdenum Electrodes In Glass-Melting Furnace
Glass & Ceramics 57 9-10 2000 333-337
C 3185
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.