Effect Of Cao And Al2O3 Addition On The Properties Of K2O-Na2O-P2O5 Glass System

This work reports the effect of substituting Al2O3 for P2O5 and substituting for (Na2O + K2O) in the ternary 0.46 (K2O + Na2O) 0.54 P2O5 glass system, with certain of these compositions being eventually of interest for biomedical applications.