Effect Of Al203 On Properties And Structure Of Lead Zinc Phosphate Glasses

Low melting lead zinc phosphate glasses have been prepared and a number of their properties evaluated. The effect of Al203 addition on the properties of these glasses has also been investigated.

Author
J Y Ding Et Al
Origin
National Lein Ho Institute, Taiwan
Journal Title
Phys Chem Glasses 43 6 2002 300-305