Edge Finishing Rectangular Glass Sheets

The edge machining of plate glass is required for the commercial and industrial use of glass sheets, to achieve an edge finish corresponding to the application, and which may extend to high-gloss polishing. According to the authors, efficient machine equipment is now available for such operations.