The Ecological Significance Of Glass Packaging In The Gdr (German)

The primary distribution systems for one-way and multi-trip bottles for the main 'end-use' sectors are reviewed, and the development of collection and recycling schemes in eastern Germany in the period 1971-1989 is analysed.

Author
U Scheunest
Origin
Unknown
Journal Title
Verpackung (Leipzeig) 1991 3 - 4 93 - 95
Sector
Container glass
Class
C 465

Request article (free for British Glass members)

The Ecological Significance Of Glass Packaging In The Gdr (German)
Verpackung (Leipzeig) 1991 3 - 4 93 - 95
C 465