Direct Current Electrical Resistivity Of Zinc Borate Glasses Containing Transition Metal Oxides

The resistivities of zinc borate glasses containing iron and vanadium oxides individually and in combination have been measured as a function of composition and temperature.

Author
R V Anavekar, N Devaraj, J Ramakrishna
Origin
Bangalore University, Indian Institute Of Science, Bangalore
Journal Title
Phys Chem Glasses 1991 32 3 103-108
Sector
Special Glass
Class
S 550

Request article (free for British Glass members)

Direct Current Electrical Resistivity Of Zinc Borate Glasses Containing Transition Metal Oxides
Phys Chem Glasses 1991 32 3 103-108
S 550