Diffusion And Permeation Constants Of Helium In Various Glasses

Measurements of the diffusion and permeation constants (and hence the solubility) of helium in different types of commercially-available glass were performed in order to investigate their suitability as materials for use in mass spectrometric systems for ultra low level tritium measurements on natural water samples.

Author
A Suckow Et Al
Origin
Universitat Hiedelberg
Journal Title
Glass Technology 1990 31 4 160-164
Sector
Special Glass
Class
S 421