Dielectric Properties Of Microporous Glass In The Microwave Region

The dielectric properties of a high-silica microporous glass were determined ar 5.5 and 11.4 GHz. Heat treatment of the glass at 800 degrees C produced a minimum dielectric constant of 2.8 and loss of 0.001.

Author
J K Yamamoto Et Al
Origin
Pennsylvania State University
Journal Title
J Am Ceram Soc 1989 72 6 916-921
Sector
Special Glass
Class
S 287

Request article (free for British Glass members)

Dielectric Properties Of Microporous Glass In The Microwave Region