Devitrification Of Li2O.5Geo2 Glass

The devitrification of Li2O.5GeO2 glass examined by differential thermal analysis and x-ray diffraction is reported and discussed.

Author
P Pernice Et Al
Origin
University Of Naples
Journal Title
Physics And Chemistry Of Glasses 33 3 June 1992 103-107
Sector
Special Glass
Class
S 651