Design Of Facades Made Of Channel Shaped Glass

After a short view on material and facade properties, this paper shows that smart facades can be built using comparatively cheap channel shaped glass. Here "Classic" systems (linear bearings at both ends of the channel shaped glass elements) as well as an own development for the facade of "Kammerspiele" in Munich is presented.