Dependence Of The Speed Of Reaction In A Glass Batch On The Physical Nature And Chemical Composition Of The Raw Materials.

By determining the amount of soda remaining in the melt, the dependence of the rate of disintegration on the grain size of sand was studied in three soda-sand batches of the same composition heated under different conditions.

Author
U. Linde And F.H. Zschacke
Origin
Unknown
Journal Title
Glastech. Ber., 11 [12] 445-54 (1933)
Sector
Primary Papers
Class
PP 882