Density Of Lead Borate Glasses In Relation To The Microstructure

The densitites of PbO-B203 glasses have been analysed to calculate the volumes of the structural units. The study presents a model to obtain the volume as a function of composition. The model makes use of the available NMR and Raman information for PbO-B203 glasses.

Author
H Doweidar & A H Oraby
Origin
Mansoura University, Egypt
Journal Title
Phys Chem Glasses 38 2 1997 69-73