Degassing Behaviour Of Optical Glasses

The suitability of high vacuum extraction to judge the fining conditions and behaviour of selected optical glasses as well as to trace the refining process in glass melting tanks is demonstated and the fining mechanism of a soda-lime-silica and of a lead-silica glass are discussed.