Decolorization Of Glass Synthesized Using Local Raw Materials

Glass samples were synthesized using raw materials from the Ural region and decolorizing agents; the chemical composition was picked as for fire-polished float glass. A glass complex additive was proposed for decolorization: cerium oxide and potassium nitrate. The spectral characteristics of the experimental glasses were studied and are presented. The maximum light transmission was reached at 750 nm and equaled 93%.

Author
L Al'Baevas & G Vlasov
Origin
Unknown
Journal Title
Glass And Ceramics 73 9 Jan/2017 361-364