Cwm 2000: A Computer-Controlled Coating System

Up to now, systems for the application of cold end coatings have been based on mechanical devices, meaning that any changes in operating conditions have had to be carried out manually and data recording of their functioning has not been an option. However, Graphoidal proposes a new approach in the form of its computer-controlled CWM 2000 (constant ware monitoring), which includes automatic adjustment and a function for feedback on system operation, among other advantages.