Energy efficient Low E glass is being successfully produce for the first time in Australia using the CVD coating process following the completion of a major upgrade at Viridian's glass making plant at Dandenong in Victoria. The commencement of the chemical Vapour Deposition (CVD) coater is the final state of the upgrade, following the successful commencement of glassmaking in October 2008.