The crystallisation of some glasses within the binary spodumene (LiAlSi206)-nepheline (NaAlSiO4) system with and without TiO2 has been investigated using X-ray diffraction analysis, scanning electron microscopy and coefficient of thermal expansion (CTE) measurements.