Crystallization Behavior Of A Glass In The Y2O3-Sio2-Aln System

Glass formation for a series of 10 glasses on or near the Y2O3-SiO2-AlN planbe of the Y-Si-Al-O-N system was found to be strongly dependent on composition with the best glass-forming characteristics occurring in a glass having a normalised composition of Y0.26Si0.30Al0.11ON0.11.

Author
T R Dinger, R S Rai, G Thomas
Origin
University Of California, Berkeley
Journal Title
J Am Ceram Soc 1988 71 4 236-244