Corrosion Tests - A Very Important Investigation Method For The Selection Of Refractories For Glass Tanks

For determining and comparing the corrosion behaviour of refractories against glass melts, a good reproducibility of the corrosion tests is needed. In this paper the reproducibility of the various most common corrosion tests, the respective procedures and the applied evaluations are discussed.