Cordierite Crystallization In Glasses Derived From The Ca0-Mg0-Al203-Si02 Quarternary System. Influence Of The Glass Composition (In Spanish)

The effect on the crystallization of cordierite for obtaining a glass-ceramic material into the Ca0-Mg0-Al203-Si02 quarternary system has been investigated.