Controlled Temperature Dryouts Of Refractory Linings

Hotwork Corp. introduced contract dryouts to the western hemisphere in 1965, many changes have occurred since then. This paper describes the process of firing castable refractories after installation using either installed burners or equipment brought in to facilitate the dryout.

Author
N W Severin
Origin
Hotwork Corp, Usa
Journal Title
Canadian Ceramics Quarterly 64 1 1995 22-23