Control Of Radioactive Waste Glass Melters: I, Preliminary General Limits At Savannah River

The melter control considerations which have been identified to facilitate compliance in the vitrification of high-level waste with the constraints imposed by processing parameters and product specifications are discussed.

Author
D F Bickford Et Al
Origin
Westinghouse Savannah River Company
Journal Title
J Amer Ceram Soc 1990 73 10 2896-2902