Continuous Chemical Tempering And Melting Innovations

In this article, the author presents details of a continuous process for chemical strengthening of glass, all-electric melting furnaces for the production of alkali-free special glass with daily pull rates of over 10 tons, and an IR-based advanced tempering technology.