Comparison Of Stress Measurement Techniques

The refractometer and polarimeter methods for measuring surface stresses in flat glass are compared by Strainoptic Technologies Inc. The benefits of residual stresses are also examined, in the light of stricter specifications for heat-strengthened and toughened glasses.