Cold-End Coatings In Glass Container Manufacture

The use of cold-end coatings in the container industry and application methods are discussed briefly with particular reference to the Emhart Powers spray mix system using a polyethylene coating material.

Author
H M Snyder
Origin
Speciality Chemicals Inc
Journal Title
Ceramic Bulletin 1990 69 11 1831-1833
Sector
Container glass
Class
C 373

Request article (free for British Glass members)