Coated Glass Processing - A Challenge For Stacking Equipment

One of the key elements for the cold end of a float line, and also for a glass processing line, are its stacking systems. This article takes a look at how one of this sector's market leaders, Grenzebach, deals with the handling of today's new coated glass types with its well-known stacking technology.

Author
E Wenninger
Origin
Grenzebach Maschinenbau, Germany
Journal Title
Glass Coatings 1/2004 12-14