Classical Nucleation Theory With A Size Dependent Interfacial Tension: Li2O.2Sio2 Crystal Nucleation

Nucleation rates for lithium disilicate are calculated as a function of temperature using a modified version of the classical nucleation theory and the results compared with experiment.

Author
M C Weinberg Et Al
Origin
University Of Arizona, Usa
Journal Title
Physics And Chemistry Of Glasses 33 3 June 1992 99-102