Chrome-Free Refractory Products For Glass Furnaces

Chrome-containing refractories are becoming environmentally undesirable. There are many alternatives available but no single one is ideal for all furnaces and conditions. This paper examines alternative options.

Author
G B Moore And I D Robertson
Origin
Hepworth Refractories Ltd
Journal Title
Glass International June 1994 17-18