Chemical And Physical Characterization Of Porous Materials Prepared By Leaching Glasses In The System Na2O-Al2O3-B2O3-F

The leachability of glasses in the system Na2O-Al2O3-B2O3-F with Al2O3 contents of about 50 wt% has been investigated.

Author
T H Elmer, T P Seward
Origin
Corning Inc
Journal Title
Glastech Ber 1991 64 1 1-8
Sector
Special Glass
Class
S 498

Request article (free for British Glass members)

Chemical And Physical Characterization Of Porous Materials Prepared By Leaching Glasses In The System Na2O-Al2O3-B2O3-F
Glastech Ber 1991 64 1 1-8
S 498
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.