Characterisation Of Graded-Index Waveguides In Glass

The results of a characterisation of graded-index waveguides obtained by silver-sodium and potassium-sodium exchange in soda-lime glasses are reported.

Author
G C Righini Et Al
Origin
Iroe-Cnr, Firenze, Universita De Selano
Journal Title
Riv Staz Sper Vetro 1990 20 6 197-200
Sector
Special Glass
Class
S 509