Calculation Of The Activation Energy Of Viscous Flow Of Alkali Silicate Glasses From Chemical Composition.

Certain quatitative relationships have been revealed between activation energy adn chemical composition of glass. The activation energy of molten glasses increases with increasing silica content in the glass.