Calcluation Of The Possibile Contents Of Opaque Glasses With Natural (Greenladn) And Synthetic Cryolite, Fluorspar, And Sodium Fluosilicate

The volatilisation of F from the glass melt is discussed, and from extensive practical experience (based on chemical analysis) constants are given for the calculation of the F content of the melted glass from a knowledge of the batch composition.

Author
F. Jcohmann.
Origin
Unknown
Journal Title
Glas-Email-Keramo-Tech., 12 [1] 6-9; [2] 41-45 (1961)
Sector
Primary Papers
Class
PP 904