Calcium Phosphates For Biomedical Applications

The history of calcium phosphates in the medicine field starts in 1769 when the first evidence of its existence in the bone tissue is discovered. Since then, the interest for calcium phosphates has increased among the scientific community. Their study has been developed in parallel with new advances in materials sciences, medicine or tissue engineering areas. Bone tissue engineering is the field where calcium phosphates have had a great importance. While the first bioceramics are selected according to bioinert, biocompatibility and mechanical properties with the aim to replace bone tissue damaged, calcium phosphates open the way to the bone tissue regeneration challenge. Nowadays, they are present in the majority of commercial products directed to repair or regenerate damaged bone tissue. Finally, in the last few decades, they have been suggested and studied as drug delivering devices and as vehicles of DNA and RNA for the future generation therapies.

Author
M Canillas Et Al
Origin
Unknown
Journal Title
Bol Soc Española Cerám Vidrio 56 3 May–June 2017 91-112 (Open Access: Https://www.Sciencedirect.com/Science/Article/Pii/S0366317517300444)
Sector
Special Glass
Class
S 4494

Request article (free for British Glass members)

Calcium Phosphates For Biomedical Applications
Bol Soc Española Cerám Vidrio 56 3 May–June 2017 91-112 (Open Access: Https://www.Sciencedirect.com/Science/Article/Pii/S0366317517300444)
S 4494
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.