Blank Inserts In Nickel Material

In this paper the author discusses how Dameron's latest designs help cut costs and improve efficiencies for glass container producers.

Author
D Baron
Origin
Dameron Alloy Foundries, Uk
Journal Title
Glass 79 2 March 2002 67