Barium & Calcium Borate Glasses As Shielding Materials For X-Rays And Gamma-Rays

Values of the y-ray, mass attenuation coefficient and the effective atomic number have been determined experimentally for xBa0.(1-x)B203(x=0.24, 0.30, 0.34, 0.40 and 0.44) and xCa0.1 (1-x)b203 (x=0.30 and 0.40) glasses at photon energies 356, 511, 662, 1173, and 1332 keV. It is pointed out that these glasses are potential radiation shielding materials. The specific volume of the glasses has been derived from density measurements and studied as a function of composition.

Author
H Singh Et Al
Origin
Guru Nanak Dev University, India
Journal Title
Phys Chem Glasses 44 1 Feb/03 5-8
Sector
Special Glass
Class
S 2516

Request article (free for British Glass members)

Barium & Calcium Borate Glasses As Shielding Materials For X-Rays And Gamma-Rays
Phys Chem Glasses 44 1 Feb/03 5-8
S 2516