This article examines the impact of a glassware ban policy on disorder-related harm within licensed premises (nightclubs) and how this action was viewed by their patrons. Field observations were conducted in a sample of eight nightclubs within Glasgow city centre.

Author
A J M Forsyth
Origin
Glasgow University, Dept Psychology
Journal Title
Alcohol & Alcoholism 43 1 2008 111-117