Automotive Glazing And New Car Trends

Glazing is a major issue in the trends of car design, and affects the spheres of electronics, alternative fuels, safety and new materials. This article deals with topics such as IR reflective solar control glass, antennas embedded into the glazing, weight reduction and stronger laminated glass, as well as increasing all-round visibility.